Cross-Linked PCross-Linked Polyolefin Shrink filmolyolefin Shrink film
Mangpaat ngagunakeun POF ngaleutikan film pikeun anjeun bisnis
Ieu bahan bungkusan serbaguna. Film ngaleutikan POF tiasa dianggo pikeun rupa-rupa produk, kalebet tuangeun, inuman, kosmétik, sareng éléktronika.
Ketebalan, lebar, sareng panjang pilem tiasa disaluyukeun ku produsén, janten cocog pikeun usaha sareng merek.
Film POF ngaleutikan kacida transparan, sahingga pamakéna gampang nempo produk jero, nu mangrupakeun titik jual signifikan pikeun usaha wanting konsumén maranéhna ningali produk saméméh purchasing.
Éta awét sareng tahan, nyegah cimata, tusukan, sareng karusakan sanésna. Éta sacara efektif tiasa ngajagi produk salami angkutan sareng neundeun.
Éta tiasa ngarangkep produk ku sababaraha cara, khususna nalika disegel ku panas, mastikeun produk di jero tetep seger sareng nahan kualitasna.
Ngajagi produk tina sababaraha faktor sapertos kalembaban, lebu, sareng rereged sanésna.
Langkung mirah ti bahan bungkusan sanés, sahingga ngahémat biaya pikeun usaha.
Film ngaleutikan POF mangrupikeun solusi bungkusan anu mangpaat pisan pikeun usaha. Kalayan sipat anu serbaguna, éta sacara efektif tiasa ngajagi produk di jero, nyiptakeun kesan anu hadé pikeun konsumén, ngabantosan dina kaputusan pameseranna. Anu paling penting, éta nawiskeun investasi anu murah dibandingkeun sareng bahan-bahan sanés, anu pasti nyayogikeun hasil anu berharga pikeun bisnis anjeun.
Parameter produk
KETEPATAN | PANJANG (M) | LEBAR(MM) | ||||||
BRJ03 | SW | CF | SW | CF | ||||
12 | 10002/6680/3334 | 1667 | 200-3200 | 150-1000 | ||||
15 | 7992/5328/2664 | 1332 | ||||||
19 | 6402/4268/2134 | 1067 | ||||||
25 | 4800/3200/1600 | 800 | ||||||
30 | 3996/2664/1332 | 666 | ||||||
38 | 3156/2104/1052 | 526 | ||||||
ID kertas inti | 76/152 | 76 | 76/152 | 76 | ||||
Poliolefin ngaleutikan Film | ||||||||
BRJ-03 | ||||||||
ITEM UJI | UNIT | UJI ASTM | NILAI KHAS | |||||
KETEPATAN | mikron | 12 | 15 | 19 | 25 | 30 | 38 | |
OPTIK | ||||||||
Halimun | D1003 | 2.2 | 2.5 | 3 | 3.7 | 4.3 | 4.5 | |
Kajelasan | D1746 | 87 | 87 | 87 | 87 | 87 | 87 | |
Gloss@45Deg | D2457 | 94 | 94 | 91 | 87 | 76 | 75 | |
SIFAT SHRINKAGE | MD | TD | MD | TD | ||||
Gratis Shrinkage 100 ℃ | % | D2732 | 15 | 25 | 15 | 25 | ||
Gratis Shrinkage 110 ℃ | % | D2732 | 35 | 45 | 30 | 40 | ||
Gratis Shrinkage 120 ℃ | % | D2732 | 68 | 70 | 65 | 66 | ||
Gratis Shrinkage 130 ℃ | % | D2732 | 81 | 80 | 80 | 79 | ||
TENSILE | ||||||||
Kakuatan Tensile (MD) | D882 | 120 | 100 | |||||
Kakuatan Tensile (TD) | 130 | 110 | ||||||
Elongation (MD) | % | 120 | 130 | |||||
Elongation (TD) | 120 | 130 | ||||||
SEAL STRENGTH | ||||||||
MD / Hot kawat Seal | N/15 mm | F88 | 12.5 | 15.2 | 18.5 | 12.5 | 15.2 | 18.5 |
TD / Seal kawat panas | 13 | 16.6 | 19 | 13 | 16.6 | 19 | ||
COF (Pilem ka Pilem) | ||||||||
Dinamis | D1894 | 0.2 | 0.2 | 0.2 | 0.2 | 0.2 | 0.2 | |
Statik | 0.21 | 0.21 | 0.21 | 0.21 | 0.21 | 0.21 | ||
Suhu Panyimpenan Max | ℃ | 32 |